Dave Fleming Posted November 7, 2018 Share Posted November 7, 2018 Painted my Harrier is Humbrol enamel 164 Dark Sea Grey (Brushed) and it’s still tacky after 4 days. Any thoughts on what to do? Link to comment Share on other sites More sharing options...
Smithy Posted November 7, 2018 Share Posted November 7, 2018 I'd put it somewhere warm and dry like the airing cupboard. I've had it happen once before with Humbrol enamels but they dried eventually. Ultimately I think you're just going to have to play the waiting game. Link to comment Share on other sites More sharing options...
Dave Fleming Posted November 7, 2018 Author Share Posted November 7, 2018 I’ll give it a try, it has been a bit cold and damp in Fife this week Link to comment Share on other sites More sharing options...
Black Knight Posted November 7, 2018 Share Posted November 7, 2018 If its a dodgy slow drying tin, add a few drops of Terebine Dryers to it. I put about 8 small drops in each tin. My enamels are dry in about 20 to 30 minutes 2 Link to comment Share on other sites More sharing options...
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now